1. Scope
1.1 This test method covers the single-point determination of the surface area of catalysts and catalyst carriers that exhibit Type II or Type IV nitrogen adsorption isotherms using a nitrogen-helium flowing gas mixture. This test method is applicable for the determination of total surface areas from 0.1 to 300 m , where rapid surface area determinations are desired.
1.2 Since the single-point method uses an approximation of the BET equation, the multipoint BET method (D3663) is preferred to the single-point method.
1.3 This standard may involve hazardous materials, operations, and equipment. This standard does not purport to address all of the safety problems associated with its use. It is the responsibility of whoever uses this standard to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
2. Referenced Documents (purchase separately) The documents listed below are referenced within the subject standard but are not provided as part of the standard.
ASTM Standards
D3663 Test Method for Surface Area of Catalysts and Catalyst Carriers
D3766 Terminology Relating to Catalysts and Catalysis
E177 Practice for Use of the Terms Precision and Bias in ASTM Test Methods
E456 Terminology Relating to Quality and Statistics
E691 Practice for Conducting an Interlaboratory Study to Determine the Precision of a Test Method
Keywords
adsorption; catalyst carriers; catalysts; continuous flow; surface area;
ICS Code
ICS Number Code 71.040.30 (Chemical reagents)
DOI: 10.1520/D4567-99
ASTM International is a member of CrossRef.